What quartz machining covers
A fused quartz part usually starts as tube, rod, plate or block and is then cut, formed and finished to a drawing. Quartz is not machined the way metal is: it is hard and brittle, it chips rather than deforms, and every operation leaves stress in the part that has to be managed before the next one. This page sets out the operations an enquiry is quoted against, and what to send so the quotation matches the drawing rather than a catalogue size.
Cutting and sawing
Tube, rod and plate are cut with diamond tooling under coolant. The decisions that get quoted are the cut finish (as-sawn or ground), the edge condition (whether a chamfer or fire-polished edge is needed), and the tolerance on length. A sawn end is a starting surface, not a sealing surface: anything that will meet another quartz part, an O-ring or a flange is normally ground or fireworked after cutting.
Bar stock dimensions decide how much finishing a finished size needs, so it is worth sending the drawing before assuming that a nominal tube size will grind down to the required wall.
Fireworking, sealing and joints
On a glass lathe the part is heated locally and formed: ends are closed or opened, tubes are joined, sockets and cones are made, flanges are attached and bends are put in. Two things belong in the enquiry here — the joint that has to hold (a ground joint, a sealed joint, or a mechanical joint with an O-ring) and the temperature the joint will see in service.
A formed or sealed part is thermally stressed where it was heated. Ask for stress relief to be stated in the quotation if the part will be cycled in a furnace, because a part that looks right on the bench can crack on the first heat-up.
Grinding, milling and drilling
Ground features carry the dimensional work: outside and inside diameters, flat faces, slots, grooves, steps and holes. Two numbers decide whether a part is straightforward or not:
- Tolerance on the feature — the site quotes ±0.05 mm as a typical figure on ground features; tighter callouts are quoted case by case, and a tight tolerance on a large thin part is a different job from the same tolerance on a short bushing.
- How it will be measured — a part that has to be inspected on a CMM or against a gauge needs datum faces the drawing names explicitly. Machining to a drawing that has no datums usually means a conversation before the quote.
Thin walls, long small-diameter bores and deep narrow slots are where a drawing gets quoted with reservations. Sending the wall thickness, the aspect ratio and the application lets that be said up front instead of after the first part is made.
Polishing and surface finish
Polished faces serve two different purposes, and they are not quoted the same way:
- Optical and sealing faces — the surface has to be free of the pits and scratches that scatter light or leak. The site quotes Ra under 0.5 µm on polished surfaces; for an optical face, state the wavelength band the part works in as well as the finish.
- Non-critical faces — a matte or as-ground finish is enough, and paying for polish there adds cost without adding function.
Say which faces are which. A drawing that marks every surface "polished" usually costs more than the application needs and delays the quote while the scope is agreed.
Cleaning and packing
Quartz is specified for purity, so what happens after machining matters as much as the machining. Cleaning is quoted to the requirement: an as-machined part for an industrial furnace and a part going into a semiconductor or analytical tool are handled differently, and the enquiry should say which one applies.
Packing follows the same rule. Bare parts wrapped in standard packaging pick up handling marks and contamination; if the part is going into a clean process, say so, because clean packing is a line item in the quotation, not a default.
Inspection and documentation
The paperwork that ships with the part is often what decides a purchase order. Tell us what is required and the quotation is built around it:
- Dimensional report against the drawing, or a first-article inspection report
- Material grade and purity documentation for the fused quartz used
- Surface finish measurement on the faces that were polished
- Certificate of conformance to the drawing revision
- Traceability of the starting material batch
Where a process requires impurity data, ICP-MS results are quoted on request. A purity figure on a data sheet and a measured impurity profile for the batch that was made are not the same document, and buyers in analytical and semiconductor work usually need the second one.
What to send with an enquiry
| Send this | Why the quotation depends on it |
|---|---|
| Drawing, with the revision number | The quote is against a revision; without one we are quoting something else |
| Tolerance callouts and datum faces | Decides the operations, the fixtures and the inspection |
| Surface finish per face, and the wavelength band if optical | Decides polish scope, which is a large part of the cost |
| Material grade, and OH content if the part sees deep UV or high temperature | Decides which fused quartz is used |
| Cleaning and packing requirement | Changes how the part is handled after machining |
| Quantity, and whether a prototype or first article is needed | Decides whether tooling is one-off or amortised |
| Service temperature and thermal cycling | Decides whether stress relief has to be specified |
If there is no drawing yet, a sketch with the critical dimensions, a photograph of the part being replaced and the application is enough to start. We will say what is missing rather than guess a dimension.
Limits worth designing around
- Brittleness — quartz does not yield. A sharp internal corner concentrates stress; a radius costs nothing to draw and is cheaper than a crack in service.
- Thermal shock — the material's low expansion is what makes it useful in furnaces, but a hot part meeting cold air or a splash still cracks. Graded warm-up and guarding belong in the design.
- Thin sections — long thin tubes and large thin plates are the parts most likely to break in handling. Where the drawing allows a thicker section, it is worth taking.
- Devitrification — surfaces that stay hot in contact with contamination go milky and lose strength. Where a part runs hot, the cleaning method and the process atmosphere matter as much as the grade.
Related components and selection guides
- Quartz tubes — the most common starting form for machined parts
- Quartz rods — supports, pins and element stock
- Quartz plates — windows, baffles and furnace supports
- Quartz tanks and boats — wet-process and furnace carriers
- Quartz heaters — emitters and replacement elements
- Quartz flanges — joints and interfaces
- Browse all quartz products
Send the drawing to sales@purequartzproducts.com or through the quote form.
Frequently asked questions
Can you machine quartz parts to a customer drawing?
Yes. The quotation is against a drawing revision: send the drawing with tolerance callouts, datum faces, the surface finish per face and the material grade. If the drawing is not finished yet, send the critical dimensions and the application — we will say what is missing rather than guess.
Can you match an existing quartz part without a drawing?
Usually, if the part is still intact enough to measure. Send the sample or clear photographs, the key dimensions (outside diameter, length, wall thickness, bore), the rating or part number if there is one, and the equipment it goes into. A dimension taken from a distorted installed part is not a reliable one, so measure out of the machine where possible.
Can a machined quartz part be made stronger by design?
On forms that distribute heat evenly, yes. A sharp corner or a sudden change of section concentrates thermal stress and is where quartz parts fail first. Adding a radius in the drawing costs nothing and is cheaper than a replacement part and a downtime window.
What documentation can ship with a machined quartz part?
State what the part needs: a dimensional report, a first-article inspection report, material purity documentation for the batch used, surface finish measurements on polished faces, a certificate of conformance to the drawing revision, and where relevant ICP-MS impurity data. These are quoted as line items, so ask for the set the purchase order actually requires rather than everything a data sheet could contain.
Why do you ask which faces need polishing?
A polished optical or sealing face is not the same as a polished decorative surface: pits and scratches scatter light and leak, so the finish on those faces is specified and measured. Marking every face as polished adds cost without adding function, and it usually delays the quote while the scope is agreed.